Skip to content

TIJ Ink Substrate Matching

The ink follows the surface, not the other way round

Most coding failures we are asked to diagnose are described as ink problems and turn out to be surface problems. The code looks acceptable on the line, then flakes, smears or disappears somewhere between the packer and the customer. Nothing was wrong with the cartridge. The ink never bonded, because the surface would not let it.

This page is the reference we use when a material is new to a line: what the surface energy of common packaging actually is, what pretreatment really changes, how fast that treatment fades, and the three tests that settle the question with tools you already have.

The one number that decides adhesion

A liquid wets a solid when the solid's surface energy is higher than the ink's surface tension — and the margin has to be comfortable. Roughly 8–10 mN/m above the ink is the working rule. A couple of units is not enough, even when it reads like a pass on paper.

That single threshold explains most adhesion complaints we are sent. Polyolefins sit below it: HDPE around 28–32 mN/m, PP around 26–28. PET sits above it at 40–42. So the same solvent ink that flakes off an untreated HDPE bottle can hold perfectly on a PET one, which is why plastic is too broad a word to choose an ink by.

Surface Surface energy Family Pretreatment usually needed
Paper, carton, corrugated, raw wood Absorbent — energy is not the limit Water-based None, normally
PP 26–28 mN/m Solvent fast-dry Commonly — corona, flame or primer
HDPE / LDPE 28–32 mN/m Solvent fast-dry Commonly — corona, flame or primer
Metallised film 32–38 mN/m Solvent fast-dry Usually
Coated or lacquered metal 30–38 mN/m Solvent fast-dry The lacquer becomes the surface you print on
Rigid PVC 38–40 mN/m Solvent fast-dry Often
PET 40–42 mN/m Solvent fast-dry Sometimes, depending on grade
Polystyrene / ABS 38–42 mN/m Solvent fast-dry Sometimes
Aluminium, uncoated High, but oxide layer is unstable Solvent fast-dry Cleanliness matters more than energy
Glass High, but chemically inert Solvent fast-dry Adhesion rides on the primer
Silicone-coated release liner Very low Not viable — no ink holds Do not print on it
Any of the above, covert marking Follows the carrier surface Covert UV Follows the carrier surface

Ranges are published industry values and general engineering rules, not measurements of your material. Surface energy moves with grade, additive package and surface state.

Three ways buyers get the surface wrong

Clear is not the same as one material. A clear bottle can be PET, PP or PVC, and the three behave completely differently under the same ink. Buying by appearance, or by the word a supplier used, is the commonest route to a failed first trial. Ask for the resin code, not the look.

Recycled content changes the surface. Post-consumer resin carries additives, residual contamination and a different additive package from virgin stock. A formulation validated on virgin HDPE is not automatically validated on a recycled grade, even when the density and melt flow match.

Additives migrate. Slip agents, antiblock and mold-release compounds are formulated to come to the surface — that is their job. When they do, the surface you print on is no longer the polymer. A batch that printed well last quarter can refuse ink this quarter without any change to the resin code.

The same logic explains why two plants using identical material can get opposite results. Treatment level, storage time, ambient humidity and the additive package all move the effective surface energy, and only one of those is printed on the bag the material arrives in.

What treatment changes, and how fast it fades

Four methods cover almost everything in packaging. They differ in how deep the change goes, how uniform it is, and how long it lasts.

Corona discharge

Raises surface energy by oxidising the top few molecular layers.

Watch for: Decays in storage. Ask for the current dyne level, not the figure on the certificate that shipped with the roll.

Flame treatment

Same effect as corona with more depth, and it tolerates thicker sections and irregular shapes.

Watch for: Heat input must be controlled. Over-treatment embrittles the surface and can create a weak boundary layer.

Chemical primer

A thin coating that becomes the surface you actually print on.

Watch for: Adds a process step and a drying step. It also moves the failure mode from the polymer to the primer.

Plasma

The most uniform option for 3D parts and small components.

Watch for: Batch equipment, so it suits formed parts rather than high-speed web.

Treatment is not permanent. Corona and flame effects decay over time as the oxidised layer reorients and low-molecular-weight material migrates back to the surface. Stock that has sat in a warehouse for months is not the same material that left the converter. When a trial fails on stored material but passes on a fresh sample, treatment decay is the first thing to check — and the fix is a dyne reading at print time, not a different cartridge.

Over-treatment is a real failure mode too. Push corona energy far enough and you build a weak boundary layer that lets the ink film lift cleanly, which reads as poor adhesion even though the surface energy number looks excellent. More treatment is not automatically better.

When the coating becomes the surface

Lacquers, varnishes, primers and label face stocks all change the question. Once a coating is present, the polymer underneath is no longer what the ink touches, and the energy value you looked up for the resin no longer applies.

Three consequences are worth carrying into a trial. A lacquer usually raises energy and improves adhesion, but it also introduces a second interface that can fail — and it will fail on the coating side, not the polymer side. A release liner or a label with a slip additive presents a deliberately low-energy face, so printing on the back of a label stock is not a formulation problem, it is a wrong-surface problem. And a matte or soft-touch coating often carries a low-energy top layer that reads as premium in the hand and repels ink completely.

Ask what the topcoat is before you ask what the ink should be. That order saves trials.

Three tests with a dyne pen, tape and water

None of these need a laboratory. Run them in this order: the water bead screens, the dyne pen measures, the tape pull confirms that the measurement translates into a bond that survives handling.

1. Dyne pen

Draw a short stroke across the surface with the lowest-numbered pen in the set, wait three seconds, and read it. If the ink holds a continuous film, that value is at or below the surface energy. If it beads into droplets within two seconds, move to the next pen down.

How to read it: You are looking for a surface energy at least 8–10 mN/m above your ink surface tension. A reading that barely passes is a failure waiting for a warm day.

2. Tape pull

Print, let the code cure for the full interval your process allows, apply standard adhesive tape over it, press firmly, and pull back at a shallow angle in one motion.

How to read it: Clean removal with no ink on the tape means adhesion is adequate. Ink transferring to the tape means the bond is weaker than the tape adhesive, which is a low bar to fail.

3. Water bead

Place a single drop of water on the surface and watch the contact angle for ten seconds.

How to read it: A drop that stays rounded and rolls off points to low energy; a drop that flattens and spreads points to a wettable surface. It is a screening test, not a measurement — use it to spot which samples deserve a dyne pen.

One discipline makes these results usable: test the material as it arrives at the print head, not as it arrives in the loading bay. A sample that has been sitting on a desk for a week is a different surface from one pulled straight off the line.

Drying is a line-layout question

Drying is not a datasheet number. What matters is where the first contact happens: the first roller, the first stacker, the first time two printed faces touch. Give us that distance and the line speed, and the drying budget becomes arithmetic.

Changing the cartridge almost never fixes a drying problem created by line layout. If the code has 300 mm and 0.4 seconds to dry before it meets a belt, a faster ink buys margin for a while, then the line runs faster and the margin disappears again. Move the print head, add a short air knife, or accept a slower ramp — those fix the cause.

Substrate to cartridge, in one table

This is the short version of everything above. Treat it as the starting point for a trial, not as a specification — your material has the final word.

Substrate Ink Pretreatment Where it usually goes wrong
Corrugated, carton, paper, wood Water-based None Lowest cost, dries fast, no odour control needed
HDPE, LDPE, PP — bottles, caps, film Solvent fast-dry Corona or flame, verified at print time The largest single group of adhesion complaints
PET — bottles, film, metallised Solvent fast-dry Depends on grade and whether the face is treated Do not assume PET behaves like the PET you used last year
Rigid PVC, PS, ABS Solvent fast-dry Often, verify per batch Additive packages vary widely between suppliers
Coated metal, lacquered cans Solvent fast-dry The coating is the surface Cleanliness of the coating decides more than the metal
Glass Solvent fast-dry Primer, usually Adhesion failures here are almost always primer or cleanliness
Any surface, mark must be invisible Covert UV Follows the carrier surface Read under 365 nm; not a readability solution

For the two cartridges this table points at, see the TIJ 2.5 solvent cartridge and the covert UV cartridge. If the surface is settled and the code still fails, the problem is usually shape rather than chemistry — folds, condensation, heat seals and abrasion are covered in choosing ink by container type.

What to send before you ask for a quote

A substrate enquiry that says plastic bottle cannot be answered well. Five details turn it into a trial that has a chance of working first time.

  1. 1 The resin code and the colour, so we can separate PET from PP from PVC.
  2. 2 Whether the face you print on is treated, and the dyne level if your converter can supply it.
  3. 3 Whether there is a lacquer, varnish or topcoat — and what it is.
  4. 4 The code content: one text line, or a 2D symbol sharing the band with one.
  5. 5 A photo of a current failure, plus the conditions it fails under.

Related reading

Get Started

READY TO SCALE
YOUR PRINT OPERATION?

Send us your printer model and monthly volume. We'll respond within 24 hours with pricing, spec sheets, and sample availability.